IRON ORE FINES AND LUMPS 

In india sea brone iron ore trade has been on the rise since the year 2002. When it was 481 MT with 7.8 % increase if touched 518 MT in 2003 and 634 MT in 2004. The world sea brone Iron ore trade has reached a new record level of 634 MT in 2004.

Chemical Composition of Indian Iron Ore Fines

  • Fe content 59.0% Rejection Below 58%
  • Fe Content 62.0% Rejection Below 61.0%
  • Fe Content 63.5% Rejection Below 62.5%
  • Silica        3.5% Max
  • Aluminia    3.5% Max
  • Sulphur     0.05% Max
  • Phos        0.07% Max

Physical Composition

  • 0 to 10 mm  90% Min
  • +10 mm       10% Max
  • Moiture         8% Max @ 105 Degree C

Calibrated Iron Ore Lumps

Chemical Composition of Calibrated Iron Ore

  • Fe Content 61.0%+ Rejection below 60.0%
  • Silica       4.0% Max
  • Aluminia   4.0% Max
  • Sulphur    0.05% Max
  • Phos        0.07% Max

Physical Size

  • 5 mm to 20 mm 90% Min (Machine Crushed and Screened)
  • Below 5 mm 10% Max
  • Tumbler Index 80+ Min

DOLOMITE Lumps and Fines

Chemical Composition of our Dolomite

  • Calcium Oxide  CaO       28.0% Min
  • Magnesium Oxide MgO   19% Min
  • Silica                          4.5% Max
  • Aluminia                      2.0% Max

Physical size Lumps (Crushed and Screened

  • 10 mm to 40mm Min 90%
  • Below 10 mm Max 10% 

Physical size Fines 

  • 0 mm to 10 mm Min 90%